Polymer Property : Compressive Strength = 0.110 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.110 MPa

@Strain 25.0 %
16.0 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..