Mechanical Properties Metric English Comments
Compressive Strength 0.150 MPa

@Strain 50.0 %
21.8 psi

@Strain 50.0 %
ISO 844
BASF Neopolen® P 8015 0.02 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Compressive Strength 0.150 MPa

@Strain 50.0 %
21.8 psi

@Strain 50.0 %
ISO 844
BASF Neopolen® P 8220 K 0.02 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Compressive Strength 0.150 MPa

@Strain 25.0 %
21.8 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 8220 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Compressive Strength 0.150 MPa

@Strain 25.0 %
21.8 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Compressive Strength 0.150 MPa

@Strain 10.0 %
21.8 psi

@Strain 10.0 %
ISO 844
BASF Neopolen® P 9035 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Compressive Strength 0.150 MPa

@Strain 10.0 %
21.8 psi

@Strain 10.0 %
ISO 844
BASF Neopolen® P 9335 MG 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Compressive Strength 0.150 MPa

@Strain 25.0 %
21.8 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Compressive Strength 0.150 MPa

@Strain 25.0 %
21.8 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 8015 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Compressive Strength 0.150 MPa

@Strain 10.0 %
21.8 psi

@Strain 10.0 %
ISO 844
BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Compressive Strength 0.150 MPa

@Strain 10.0 %
21.8 psi

@Strain 10.0 %
ISO 844
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..