Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 8015 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9035 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9230 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9435 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to..
Compressive Strength 0.220 MPa

@Strain 25.0 %
31.9 psi

@Strain 25.0 %
ISO 844
BASF Neopolen® P 8220 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Copyright © lookpolymers.com All Rights Reserved