Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 10.3 MPa @Temperature 110 °C, Time 86400 sec |
1490 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories AU1 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 10.3 MPa @Temperature 1371 °C |
1490 psi @Temperature 2500 °F |
Cold Crush Strength |
BNZ Materials Blazecrete 3000 G Dense Castable Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc. |
|||
Compressive Strength | 10.3 MPa @Treatment Temp. 104 °C |
1500 psi @Treatment Temp. 219 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Bazelite 2500 LI Insulating Castable Blaz 2500 LI is an extremely strong insulating castable designed for general purpose use in those areas that require this combination of light weight and high strength, such as forge furnace doors a.. |