Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0800 MPa @Strain 25.0 % |
11.6 psi @Strain 25.0 % |
ISO 844 |
BASF Neopolen® P 8015 0.02 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |
|||
Compressive Strength | 0.0800 MPa @Strain 25.0 % |
11.6 psi @Strain 25.0 % |
ISO 844 |
BASF Neopolen® P 8220 K 0.02 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |