Compressive Strength 7.85 MPa

@Temperature 800 °C
1140 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 1.4 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories APC-120G Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories TD-R75 Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).