Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 820 MPa @Temperature 82.2 °C |
119000 psi @Temperature 180 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Compressive Strength | 820 MPa @Temperature 23.9 °C |
119000 psi @Temperature 75.0 °F |
Dry, 365° Oven Cured; SACMA 1R-94 |