Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 122 MPa @Strain 5 % |
17700 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data) This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi.. |