Polymer Property : Compressive Strength = 133.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 133.0 MPa

@Temperature 850 °C
19290 psi

@Temperature 1560 °F
after Firing; ASTM C-349
Stellar Canada CERAMITE® CSR-S Wear Resistant Castable
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w..