Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 145 MPa @Strain 5 % |
21000 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data) Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo.. |
|||
Compressive Strength | 145 MPa @Strain 5 % |
21000 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Compressive Strength | 145 MPa @Temperature 23.0 °C |
21000 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Compressive Strength | 145 MPa @Temperature 120 °C |
21000 psi @Temperature 248 °F |
ISO 604 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Compressive Strength | 145 MPa @Strain 5 % |
21000 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data) This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap.. |