Polymer Property : Compressive Strength = 18.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 18.5 MPa

@Strain 2 %
2680 psi

@Strain 2 %
ISO 604
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data)
This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to..