Compressive Strength 124 MPa

@Temperature 87.8 °C
18000 psi

@Temperature 190 °F
Wet (2hr water boil immersion); ASTM D695
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Compressive Strength 124 MPa

@Temperature 200 °C
18000 psi

@Temperature 392 °F
ASTM D-695
Glastic GLASTHERM HT200 Insulation Sheet
HT200 features:High Hot Compressive StrengthLow Thermal ConductivityOil and Moisture ResistantReduces Heat LossHelps Control TemperatureFaster Mold StartupDesigned for reducing heat losses from plas..
Compressive Strength 124 MPa

@Temperature 200 °C
18000 psi

@Temperature 392 °F
ASTM D-695
Glastic GLASTHERM HT Insulation Sheet
Glastherm Grade HT is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT is completely as..