Mechanical Properties Metric English Comments
Compressive Strength 188 MPa

@Temperature 23.0 °C
27300 psi

@Temperature 73.4 °F
JIS K7208
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Compressive Strength 188 MPa

@Temperature 22.8 °C
27300 psi

@Temperature 73.0 °F
JIS K7208
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled  (discontinued **)
AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber ..