Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 110 - 130 MPa @Temperature 1000 °C |
16000 - 18900 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Compressive Strength | 110 - 130 MPa @Temperature 1300 °C |
16000 - 18900 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 G Dense Vibrating Refractory Castable Description: Vibron 150 G is a low cement castable based on sintered South-American bauxite. Especially suited for direct contact with liquid aluminum metal.Remarks: Indicated values apply to vibrat.. |