Polymer Property : Compressive Strength = 200 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 200 MPa

@Temperature 23.9 °C
29000 psi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Compressive Strength 200 MPa

@Temperature 120 °C
29000 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Compressive Strength 200 MPa

@Temperature 120 °C
29000 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Compressive Strength 200 MPa

@Temperature 120 °C
29000 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
Compressive Strength 200 MPa

@Temperature 120 °C
29000 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Compressive Strength 200 MPa

@Temperature 200 °C
29000 psi

@Temperature 392 °F
Elisto THERMOSTAR® HD 800 Frame Press Insulation Material
Pattern material. Insulation materials for mechanical engineering.Information provided by elisto
Compressive Strength 200 MPa

@Temperature 23.0 °C
29000 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..