Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 155 MPa @Temperature 120 °C |
22500 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Compressive Strength | 155 MPa @Temperature 23.0 °C |
22500 psi @Temperature 73.4 °F |
ASTM D 695 |
Saint-Gobain Meldin® 1003 Thermoplastic Bearing Material Meldin 1003 components offer the highest level of strength and rigidity for this product family. They maintain high chemical, tensile, and flexural properties even at elevated temperatures.MeldinÂ.. |
|||
Compressive Strength | 155 MPa @Strain 5 % |
22500 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |