Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-140 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 110 °C, Time 86400 sec |
2130 - 3560 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1000 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1000 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 110 °C, Time 86400 sec |
2130 - 3560 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |