Polymer Property : Compressive Strength = 2560 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 9.81 - 17.7 MPa

@Temperature 1300 °C,
Time 10800 sec
1420 - 2560 psi

@Temperature 2370 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PTC-130S Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).