Mechanical Properties Metric English Comments
Compressive Strength 21.6 MPa

@Temperature 800 °C
3130 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics Sharada AIO-SiC-C Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..