Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 324 MPa @Temperature 71.1 °C |
47000 psi @Temperature 160 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 324 MPa @Temperature 71.1 °C |
47000 psi @Temperature 160 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 324 MPa @Temperature 23.9 °C |
47000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi.. |
|||
Compressive Strength | 324 MPa @Temperature 288 °C |
47000 psi @Temperature 550 °F |
Dry |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ S2-Glass Fabric MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e.. |