Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 23.4 MPa @Temperature 204 °C |
3390 psi @Temperature 399 °F |
ASTM D 695 |
Saint-Gobain Meldin® 1003 Thermoplastic Bearing Material Meldin 1003 components offer the highest level of strength and rigidity for this product family. They maintain high chemical, tensile, and flexural properties even at elevated temperatures.MeldinÂ.. |
|||
Compressive Strength | 23.4 MPa @Temperature 1260 °C |
3390 psi @Temperature 2300 °F |
Cold Crush Strength |
BNZ Materials Blazecrete 2500 HS Dense Castable Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li.. |