Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 372 MPa @Temperature 23.9 °C |
54000 psi @Temperature 75.0 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:.. |
|||
Compressive Strength | 372 MPa @Temperature 149 °C |
54000 psi @Temperature 300 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |