Compressive Strength 38.6 MPa

@Temperature 815 °C
5600 psi

@Temperature 1500 °F
Cold Crush Strength
BNZ Materials Blazecrete 2500 HS Dense Castable
Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li..