Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.96 - 4.41 MPa @Temperature 1000 °C, Time 10800 sec |
284 - 640 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories GUN-140L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 2.94 - 4.41 MPa @Temperature 110 °C, Time 86400 sec |
427 - 640 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories GUN-80L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 2.45 - 4.41 MPa @Temperature 1000 °C, Time 10800 sec |
356 - 640 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories GUN-135L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |