Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 4.83 MPa @Treatment Temp. 104 °C |
700 psi @Treatment Temp. 219 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Bazelite 2300 LI Insulating Castable Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u.. |
|||
Compressive Strength | 4.83 MPa @Temperature 815 °C |
700 psi @Temperature 1500 °F |
Cold Crush Strength |
BNZ Materials Bazelite 2600 LI Insulating Castable Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov.. |
|||
Compressive Strength | 4.83 MPa @Temperature 1095 °C |
700 psi @Temperature 2003 °F |
Cold Crush Strength |
BNZ Materials Bazelite 2600 LI Insulating Castable Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov.. |
|||
Compressive Strength | 4.83 MPa @Temperature 1260 °C |
700 psi @Temperature 2300 °F |
Cold Crush Strength |
BNZ Materials Bazelite 2600 LI Insulating Castable Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov.. |
|||
Compressive Strength | 4.83 MPa @Temperature 1371 °C |
700 psi @Temperature 2500 °F |
Cold Crush Strength |
BNZ Materials Bazelite 2600 LI Insulating Castable Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov.. |
|||
Compressive Strength | 4.83 MPa @Treatment Temp. 104 °C |
700 psi @Treatment Temp. 219 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Bazelite 2600 LI Insulating Castable Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov.. |