Compressive Strength 280 MPa

@Strain 5 %
40600 psi

@Strain 5 %
ISO 604
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data)
Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic..
Compressive Strength 280 MPa

@Temperature 23.0 °C
40600 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant..
Compressive Strength 280 MPa

@Temperature 200 °C
40600 psi

@Temperature 392 °F
ASTM D-695
Glastic GLASTHERM HT220 Insulation Sheet
Glastherm Grade HT220 is a thermal insulation sheet that is a highly heat-resistant material that combines low thermal conductivity with very high compressive strength at molding temperature. It is..
Compressive Strength 280 MPa

@Temperature 200 °C
40600 psi

@Temperature 392 °F
Elisto THERMOSTAR® LC 610 Insulation Material
Pattern material. Insulation materials for mechanical engineering.Information provided by elisto