Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 41.0 MPa @Strain 2 % |
5950 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data) Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro.. |