Polymer Property : Compressive Strength = 4190 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 28.9 MPa

@Treatment Temp. 104 °C
4190 psi

@Treatment Temp. 219 °F
Cold Crush Strength; Dried 104°C
BNZ Materials Blazecrete 3000 Dense Castable
Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec..