Compressive Strength 48.8 MPa

@Temperature 1556 °C
7080 psi

@Temperature 2833 °F
Cold Crush Strength; At Use Limit
BNZ Materials Blazecrete 2800 Dense Castable
Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur..