Polymer Property : Compressive Strength = 52000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 359 MPa

@Temperature 177 °C
52000 psi

@Temperature 350 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Compressive Strength 359 MPa

@Temperature 216 °C
52000 psi

@Temperature 420 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Compressive Strength 359 MPa

@Temperature 93.3 °C
52000 psi

@Temperature 200 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Strength 359 MPa

@Temperature 93.3 °C
52000 psi

@Temperature 200 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Strength 359 MPa

@Temperature 82.2 °C
52000 psi

@Temperature 180 °F
Wet; Vacuum/Oven Cured; SACMA 1-94
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Compressive Strength 359 MPa

@Temperature 288 °C
52000 psi

@Temperature 550 °F
Dry
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric
MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e..