Mechanical Properties Metric English Comments
Compressive Strength 44.1 - 53.9 MPa

@Temperature 1500 °C,
Time 10800 sec
6400 - 7820 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-180 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).