Mechanical Properties Metric English Comments
Compressive Strength 36.8 MPa

@Temperature 1100 °C
5330 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics REFCAST 80 High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..