Compressive Strength 37.7 MPa

@Temperature 1100 °C,
Time 10800 sec
5460 psi

@Temperature 2010 °F,
Time 3.00 hour
Cold Crushing, Typical Value, After firing @ 1100°C
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic
Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd.