Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 55.2 MPa @Treatment Temp. 104 °C |
8010 psi @Treatment Temp. 219 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Blazecrete 2500 HS Dense Castable Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li.. |