Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 550 MPa @Thickness >=5.00 mm, Temperature 100 °C |
79800 psi @Thickness >=0.197 in, Temperature 212 °F |
Perpendicular to laminations; EN 60893 |
HOS-Technik Homide 250 Bismaleimide Resin Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel.. |