Mechanical Properties Metric English Comments
Compressive Strength 380 MPa

@Temperature 150 °C
55100 psi

@Temperature 302 °F
ASTM D-695
Glastic GLASTHERM HT220 Insulation Sheet
Glastherm Grade HT220 is a thermal insulation sheet that is a highly heat-resistant material that combines low thermal conductivity with very high compressive strength at molding temperature. It is..