Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 565 MPa @Temperature 21.1 °C |
82000 psi @Temperature 70.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 565 MPa @Temperature 82.2 °C |
82000 psi @Temperature 180 °F |
Dry; Autoclave Cured; SACMA 1-94 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |