Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 57.9 MPa @Temperature 1500 °C, Time 10800 sec |
8390 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CTL ASP-S Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 57.9 MPa @Treatment Temp. 104 °C |
8400 psi @Treatment Temp. 219 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |