Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 4.00 MPa @Strain 1 % |
580 psi @Strain 1 % |
ISO 604 |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |