Polymer Property : Compressive Strength = 65.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 65.7 MPa

@Temperature 1500 °C,
Time 10800 sec
9530 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-16 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).