Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 527 MPa @Temperature 23.9 °C |
76400 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® P-600 Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processingKey Features and Benefits:Meets MIL-R-7575 requirements160.. |