Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 660 MPa @Temperature >=21.1 °C |
95700 psi @Temperature >=70.0 °F |
Dry, 0° Direction, Ultimate |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |