Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 986 MPa @Temperature 21.1 °C |
143000 psi @Temperature 70.0 °F |
Test at RT after Oxidative Stability Test (600°F, 150 psia, 121 hrs) |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ IM7 12K Carbon Unitape MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-.. |