Mechanical Properties Metric English Comments
Compressive Modulus 0.00140 GPa

@Strain 20.0 %
0.203 ksi

@Strain 20.0 %
Vicone High Performance Rubber VicoSilâ„¢ KC605Q-OR High Performance Silicone Rubber
Information provided by Vicone