Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00153 GPa @Strain 20.0 % |
0.222 ksi @Strain 20.0 % |
|
Vicone High Performance Rubber VicoSealâ„¢ 106C-BK High Performance EPDM Rubber Information provided by Vicone |