Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 145 GPa @Temperature 23.9 °C |
21100 ksi @Temperature 75.0 °F |
Dry, 365° Autoclave Cured; SACMA 1R-94 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, IM7 Unitape Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Compressive Modulus | 145 GPa @Temperature 82.0 °C |
21000 ksi @Temperature 180 °F |
0°, Dry |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Compressive Modulus | 145 GPa @Temperature 23.0 °C |
21000 ksi @Temperature 73.4 °F |
[0°]; Resin Content=29%, Fiber Volume=64% |
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel |