Mechanical Properties Metric English Comments
Compressive Modulus 20.7 GPa

@Temperature 87.8 °C
3000 ksi

@Temperature 190 °F
Wet (2hr water boil immersion); ASTM D695
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Compressive Modulus 20.7 GPa

@Temperature 71.1 °C
3000 ksi

@Temperature 160 °F
Wet; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 20.7 GPa

@Temperature 260 °C
3000 ksi

@Temperature 500 °F
Dry; 325°F Autoclave Cured; ASTM D695
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Compressive Modulus 20.7 GPa

@Temperature 121 °C
3000 ksi

@Temperature 250 °F
Dry; ASTM D695
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi..
Compressive Modulus 20.7 GPa

@Temperature 24.0 °C
3000 ksi

@Temperature 75.2 °F
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F155; Fiber: 450-1/2Information provided by HexCel
Compressive Modulus 20.7 GPa

@Temperature 71.0 °C
3000 ksi

@Temperature 160 °F
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric
Information provided by HexCel