Polymer Property : Compressive Modulus = 22.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 22.8 GPa

@Temperature 23.9 °C
3300 ksi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Compressive Modulus 22.8 GPa

@Temperature 21.1 °C
3300 ksi

@Temperature 70.0 °F
Wet; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 22.8 GPa

@Temperature -53.9 °C
3300 ksi

@Temperature -65.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 22.8 GPa

@Temperature 23.9 °C
3300 ksi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Compressive Modulus 22.8 GPa

@Temperature 177 °C
3310 ksi

@Temperature 351 °F
Hexcel® F161 Epoxy Resin, 1581 Glass Fabric
Hexcel designation: 1581-38"-F161; Fiber: 150-1/2Information provided by HexCel