Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 20.0 GPa @Temperature 93.3 °C |
2900 ksi @Temperature 200 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 20.0 GPa @Temperature 21.1 °C |
2900 ksi @Temperature 70.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 20.0 GPa @Temperature 177 °C |
2900 ksi @Temperature 351 °F |
|
Hexcel® F161 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F161; Fiber: 450-1/2Information provided by HexCel |