Mechanical Properties Metric English Comments
Compressive Modulus 31.0 GPa

@Temperature 177 °C
4500 ksi

@Temperature 351 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric
Information provided by HexCel